Pl see appendix X2 of ASTM A193 which highlights the coating and application limits with regard to temperature and possibilities of liquid and solid metal embrittlement.

Regards
Shyam

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kadam Vijay (Mumbai - Piping)
Sent: venerdì 4 settembre 2009 10.09
To: materials-welding@googlegroups.com
Subject: [MW:3115] material resistance temperature for Zinc plated bolting.


Dear All,

In our project we have requirement of Zinc-Plating / bichromate-treated on bolting in carbon steel & P11 piping class.
Now Max. Design Temp in P11 piping classes is 405 DegC & 200 DegC in carbon steel classes.

I want to know the max temperature upto which zinc plated bolting can be used & if zinc plating is not suitable for this temp other alternative plating type.

Thank you for your kindly help.


Kind Regards,
Vijay Kadam

******************************************************************************************
CONFIDENTIALITY NOTICE
This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...