[MW:2837] Re: 2827] AWS-CWI best agency in INDIA

HI All,
It all depends upon the tutor and the materials which he
gives during the class.

Regards,
Y.C.Shiva,
QA/QC Engineer,
Certified Inspector API 653,570, CSWIP 3.1, NACE CIP lev 2,
Doha Qatar.

On 7/28/09, SLM <smahuri@lntecc.com> wrote:
> Yes, you have rightly heard.
>
> Among the four listed agencies IQC is the best. As most of my friends have
> completed this course successfully through IQC only.
> So you can opt for IQC.
>
>
> Thanks and Regards,
>
> Snehkumar L Mahuri
> Regional Quality Manager
> HC&P (Vertical)
>
> M : 9428819849
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of
> PREMSHANKARDUTTNAUTIYAL
> Sent: Tuesday, July 28, 2009 9:04 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:2827] AWS-CWI best agency in INDIA
>
> Hi Friends
>
> I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course
> + Exam in the next couple of months. But in India there are 4 AWS approved
> agencies which conduct this AWS course.I am confused as to which agency i
> should select as i have to invest a huge amount of money... .
>
> 1)Industrial Quality Concepts
> Address: IQC Training & Services, Pte, Ltd
> Shivani Block -1, Ist Floor
> 40 East Coast Road
> Chennai, India 600041
> Telephone: 91-44-42158714/42158715/24451009
> Fax Number: 91-44-5215-8715
> Email: iqc.in.org@vsnl.com
> Contacts: Sundaran Baskaran
>
> 2)BETZ Engineering & Technology Zone
> Address: 49-Vellalar Street
> Near St Thomas Mount Railway Station
> Chennai - 600088
> INDIA
> Tel: 91-44-65364123/22441234
> TeleFax: 91-44-22441234
> Email: betzzone@vsnl.net
> Site: www.betzinternational.com
>
> 3)DASH Inspectorate
> Address: 3rd Floor,Iswar Krupa Building Near Bank Of India,
> Saffron Circle,Fatehgunj,
> Baroda-390002,Gujarat,India
> Phone: +91 265 2750116, 3017474
> Fax: +91 265 2788278
> Site: www.dashinspectorate.com
>
> 4)Agency: Moody ICL Certifications Limited
> Address: #372, Industrial Area Phase I
> Panchkula
> Haryana
> India
> PIN 134112
> Website: www.moodyint.com
>
> Hence can anyone guide me from their past experience as to which agency is
> the best. Please give your unbiased opinion..
> I have heard from all my colleagues that IQC,chennai is the best and most
> experienced in conducting CWI.
>
> Please guide me to select the best agency which will provide good
> preparatory training.
>
> Regards
>
> Prem Nautiyal
> Mumbai.
>
> PREM S NAUTIYAL
>
> CELL : 9820313278
> [http://sigads.rediff.com/RealMedia/ads/adstream_nx.ads/www.rediffmail.com/signatureline.htm@Middle]<http://sigads.rediff.com/RealMedia/ads/click_nx.ads/www.rediffmail.com/signatureline.htm@Middle?></Table
>
>
>
>
>
> ________________________________
> "This Message and its contents is intended solely for the addressee and is
> proprietary.Information in this mail is for L&T Business Usage only. Any Use
> to other than the addressee is misuse and infringement to Proprietorship of
> L&T ECC.If you are not the addressee please return the mail to the
> sender.L&T ECC DIVISION"
>
> >
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...