Skip to main content

[MW:2843] RE: 2839] Re: AWS-CWI best agency in INDIA

Can you please give the address and contact numbers for IANT ( Institute of Advanced NDT Technology)?

 

 

Regards

 

Chandulal S Vithlani

--------------------------------------------------------------------

Dear Prem,
I suggest you that if you are planning to attend AWS for Overseas job opportunities then please think about CSWIP 3.1 welding Inspector.
main difference : AWS validity - 3 years.
                         CSWIP 3.1 - Validity 5 years
AWS membership compulsory. every year you have to pay.
CSWIP membership not compulsory.
Renewal - AWS = INR 22000/- after three years CSWIP 3.1 = INR 15,000/-

Choice is yours! - CSWIP 3.1 = Tata Projects limited.
and for Preparatory courses IANT ( Institute of Advanced NDT Technology)

Regards,
Nilesh

On Tue, Jul 28, 2009 at 4:33 AM, PREMSHANKARDUTTNAUTIYAL <prem_nautiyal@rediffmail.com> wrote:

Hi Friends

I stay in Mumbai and have prepared for AWS-CWI and want to appear for Course + Exam in the next couple of months. But in India there are 4 AWS approved agencies which conduct this AWS course.I am confused as to which agency i should select as i have to invest a huge amount of money... .

1)Industrial Quality Concepts
Address: IQC Training & Services, Pte, Ltd
Shivani Block -1, Ist Floor
40 East Coast Road
Chennai, India 600041
Telephone: 91-44-42158714/42158715/24451009
Fax Number: 91-44-5215-8715
Email: iqc.in.org@vsnl.com
Contacts: Sundaran Baskaran

2)BETZ Engineering & Technology Zone
Address: 49-Vellalar Street
Near St Thomas Mount Railway Station
Chennai - 600088
INDIA
Tel: 91-44-65364123/22441234
TeleFax: 91-44-22441234
Email: betzzone@vsnl.net
Site: www.betzinternational.com

3)DASH Inspectorate
Address: 3rd Floor,Iswar Krupa Building Near Bank Of India,
Saffron Circle,Fatehgunj,
Baroda-390002,Gujarat,India
Phone: +91 265 2750116, 3017474
Fax: +91 265 2788278
Site: www.dashinspectorate.com

4)Agency: Moody ICL Certifications Limited
Address: #372, Industrial Area Phase I
Panchkula
Haryana
India
PIN 134112
Website: www.moodyint.com

Hence can anyone guide me from their past experience as to which agency is the best. Please give your unbiased opinion..
I have heard from all my colleagues that IQC,chennai is the best and most experienced in conducting CWI.

Please guide me to select the best agency which will provide good preparatory training.

Regards

Prem Nautiyal
Mumbai.

PREM S NAUTIYAL

CELL : 9820313278

 




--
Best Regards,

Nilesh Pathare


**********************************************************************

Borouge is a leading provider of value creating, innovative plastics solutions for customers in the Middle East, Asia-Pacific and Africa. Borouge employs unique Borstar® technology to produce differentiated products for high-value infrastructure applications, including water, gas and industrial pipe systems, power and communication cables, advanced packaging and automotive components. Borouge's state-of-the-art petrochemical complex is located at Ruwais, Abu Dhabi in the United Arab Emirates.

===================================================================================
CONFIDENTIALITY NOTICE

This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please delete the email and any attachment(s) and notify the sender.

This footnote also confirms that this email message has been scanned for the presence of computer viruses.
=============================================================================================================

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...