Skip to main content

[MW:2735] RE: 2733] RE: 2729] Ferrite Number (FN) for the deposited weld metal

Thanks  Mr. Hegde,

Can heat input , be a variable for erratic ferrite no ?

For example I’m using filler wire of the same batch no ( packet ) & welder , but in one joint I get Ferrite no. less than 8 % and in other joint I get over 10%.

 

Best Regards,

Rishi Raj Singh


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PB HEGDE
Sent: Tuesday, July 21, 2009 1:57 PM
To: materials-welding@googlegroups.com
Subject: [MW:2733] RE: 2729] Ferrite Number (FN) for the deposited weld metal

 

 

 

Austenetic SS used in chemical /petrochemical plant require  good Corrosion resistance. For which delta ferrite plays the major role.

i)Increase in Delta Ferrite will reduce the corrosion resistance . Therefore in severe corrosion resistance requirement  , ferrite to be kept below 8% (Generally it is kept between  3-7 %)However  very low ferrite  causes defect like hot crack, fissures ,There is no code requirement but Ferrite requirement is decided by process licenser ,depending upon the service condition

ii)You can check ferrite No by Instrument called Ferrite Meter where you can get Ferrite No directly ,Some time You can check with respect to Delong Diagram ( Given in ASME Sec 2C ) by calculating /plotting the Cr , and Ni equivalent from actual chemical analysis of weld  

iii)My experience –some time Ferrite no increases due to work hardening of material If you measure by Ferrite meter

Regards

 

Hegde P.B.

09714714803

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of tong tong
Sent: Monday, July 20, 2009 9:31 AM
To: materials-welding@googlegroups.com
Subject: [MW:2729] Ferrite Number (FN) for the deposited weld metal

 

Dear All,

Regarding above mentioned subject, i would like to know in detail about ferrite number. I have a few questions to ask such as What is the ferrite number? Why it is so important? Materials subjected to ferrite number? Permissible limit of ferrite number? Code and standard that we refer to requirement of ferrite number? Procedure to perform ferrite number?..If anybody have experience or information regarding this subject hopefully you can share with me. Thank in advance for your kind cooperation


Regards
tong2



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...