[MW:2800] Re: Additional Welding layers

It´s ok, don´t vworry you are below the maximun thickness qualificated
Antonio Ruscitto

>>> Mohamed Mubarak Syed <smmubarakqc@gmail.com> 23/07/2009 10:02 am >>>
Can any one clarify,
 
We have appproved WPS Which is showing  8 passes, to cover the thickness of PQR apecimen (12.7 mm), But thickness range is 6.9mm to 19.1mm, We have production welding thickness is 18 mm,
 
So we need to do additional weld passes to cover the required thickness, approximately 12 passes in production welding
 
Kindly advice

*********************************************************************

¡IMPORTANTE!

Para evitar accidentes por inhalación de monóxido de carbono:

- Mantenga los ambientes ventilados en forma permanente.

- Revise que la llama sea color azul y uniforme.

- Instale y haga revisar periódicamente sus artefactos sólo a través de gasistas matriculados.

Recuerde que los artefactos a gas pueden emitir Monóxido de Carbono: un gas altamente tóxico e imperceptible.

Más consejos en http://www.metrogas.com.ar

*********************************************************************

Este mensaje es privado y confidencial y va dirigido sólo al destinatario indicado. Si lo ha recibido por error, por favor avísenos inmediatamente vía e-mail a error-mail@metrogas.com.ar y tenga la amabilidad de eliminarlo de su sistema. La utilización o divulgación de su contenido puede importar la comisión de un delito. No copie, reproduzca o divulgue -en forma parcial o total- su contenido. Cualquier opinión contenida, es exclusiva de su autor y no representa la opinión de MetroGAS S.A. - Muchas gracias.

This message is private and confidential and it is only intended for the addressee named above. If you have received this message and it is not addressed to you, please advise us immediately at error-mail@metrogas.com.ar and kindly remove it from your system. The use or disclosure of its contents may be regarded as an offense. Do not copy, reproduce or disclose them, either partially or fully. Opinions are the exclusive responsibility of the author and do not represent the opinion of MetroGAS S.A. - Thank you.

:: http://www.metrogas.com.ar

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...