[MW:1659] Re: A333 Material for impact test requirement

First of all, let me clarify that A333 material is intended for low
temperature service only. So it is unlikely that the material is not impact
tested except for grade-11

ASTM A333 calls for impact testing (except grade-11) as per the material
standard itself when the thickness exceeds 3 mm. (Refer Para-8 and
Table-5).

So far as the impact testing of material (as per design standard) is
concerned, I feel it is very well explained in Para 323.2.2(particularly
sub para a) and Table 323.2.2. Other/subsequent para's are also elaborative
for the exact requirement for various materials. Also, refer the Fig.
323.2.2A for other materials.

I hope this has clarified. As a matter of fact, I could not follow your
exact question. If you have any particular doubt, pl. specify otherwise, it
seems to be a hypothetical question.

Best regards,

Prasad


"Faigal Fernando
Agbanawag"
<faigal.agbanawag To
@czfp.com> <materials-welding@googlegroups.com
Sent by: >
materials-welding cc
@googlegroups.com
Subject
[MW:1655] A333 Material for impact
26/02/09 04:06 PM test requirement


Please respond to
materials-welding
@googlegroups.com


Dear all,

Can anybody elaborate chapter III of B31.3 regarding the impact test
requirement of ASTM A333 where in section 323.2.2 states the limitation
concerning impact testing of a particular material. Is it mandatory for
A333 to have an impact test ?, where low temperature service is not an
issue.

Your response are highly appreciated.

Regards,

Faigal Fernando Agbanawag
Sr. Piping Engineer
Clough ZFP



T +966 3 8828818 Ext: 241

F +966 3 8828622

M +966 (0) 507780576


Disclaimer: This email and any files transmitted with it are confidential
and intended solely for the use of the addressee(s) named herein. If you
are not the intended recipient or addressee, you should not use,
disseminate, distribute, copy or alter this email. Any views or opinions
presented in this email are solely those of the author and might not
represent those of "CZFP".


Warning: Although reasonable precautions have been taken to ensure no
viruses are present in this email, "CZFP" cannot accept responsibility for
any loss or damage arising from the use of this email or attachments. If
you have received this electronic mail message in error, please contact the
sender directly.


Save a tree...please don't print this e-mail unless you really need to.

Save a tree...please don't print this e-mail unless you really need to.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...