[MW:1618] Re: WPS from 2 PQRs

Dear VJ

I could not understand the exact question. There is no contradiction in the
two para's QW 200.2/200.4 as mentioned by you. Rather, 200.2 is general
rule, while QW200.4 specifies the specific requirements of preparation of
WPS using more than one PQR (QW 200.4/a) and specific
relaxations/requirements root runs (QW 200.4/b). In any case, the essential
and supplementary essential variables (when required) are required to be
supported by PQR.

Please elaborate your question, if in doubt.

Best regards,

Prasad


VJ V
<veevee17@gmail.c
om> To
Sent by: "Materials & Welding"
materials-welding <materials-welding@googlegroups.com
@googlegroups.com >
cc

24/02/09 11:02 AM Subject
[MW:1617] WPS from 2 PQRs

Please respond to
materials-welding
@googlegroups.com

Hi everyone,

I would like to know reg Sec IX,QW 200.2(f) and QW 200.4(a)

200.2(f) states " A single WPS may cover several essential variable
changes......(eg. a single WPS may cover a thinkness range from 1.5mm
thru 32mm if PQR exist for both 1.5 to 5mm and 5mm thru 32 mm ranges)

But QW 200.4(a) states if all essential/supplementary essential
variable according to QW 451 is meeting then ......

My doubt is this: As per 200.2(f), "Base metal range" is not meeting
the requirement of QW 451.

But QW 200.4(a), states base metal thickness range, weld metal
thickness range etc shall meet QW 451.

Can anybody please clarify...

Regrds


Save a tree...please don't print this e-mail unless you really need to.

Save a tree...please don't print this e-mail unless you really need to.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---