                     What is the grade of pipe? Is it conforms to API 5L or ASTM A106.? For API 5L you have to refer section 7.8.14. For ASTM A106 you have to refer section 18.2 & 18.3.1
 
Regards
Prabhakar. S

 
On 1/31/09, sadique sheikh <mails_sadique@yahoo.com> wrote:
can u tell me about the acceptance limit of dent in piping also in which section of asme should i get the specification of dent of piping?

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...