Dear Sadique
The joint sketch which you have shown is a double bevel groove + fillet joint.
In order to know the fusion of plate A with plate B, you have to use a normal beam probe and scan from the back of Plate A if accessible.
What are the plate thicknesses ??
Regards
Prem Nautiyal
On Mon, 03 Jan 2011 16:36:24 +0530 wrote
>Actually I want to know the defect of incomplete fusion in T-joint
fillet weld.Please see attached Drawing for reference. In that Can we
know about fusion on plate A with welding with angle probe or we must
need TR probe to identify the defect? Bevel angle side fusion we get
with angle probe.
On Mon, Jan 3, 2011 at 2:51 PM, muthusrinivasan muthuselvam
wrote:
> Dear Mr.Sadique..
>
> what you are looking exactly in fillet weld UT..
>
> Can you elaborate little bit..
>
> br,
> msms
>
> On Mon, Jan 3, 2011 at 1:40 PM, Sadique Sheikh wrote:
>>
>> Dear All,
>> During UT inspection of fillet weld, Does we need both angle probe and
>> normal or TR probe?
>>
>> Thanks & Regards,
>> Mohd. Sadique Sheikh
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
PREM S NAUTIYAL
CELL : 9769316004
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
The joint sketch which you have shown is a double bevel groove + fillet joint.
In order to know the fusion of plate A with plate B, you have to use a normal beam probe and scan from the back of Plate A if accessible.
What are the plate thicknesses ??
Regards
Prem Nautiyal
On Mon, 03 Jan 2011 16:36:24 +0530 wrote
>Actually I want to know the defect of incomplete fusion in T-joint
fillet weld.Please see attached Drawing for reference. In that Can we
know about fusion on plate A with welding with angle probe or we must
need TR probe to identify the defect? Bevel angle side fusion we get
with angle probe.
On Mon, Jan 3, 2011 at 2:51 PM, muthusrinivasan muthuselvam
> Dear Mr.Sadique..
>
> what you are looking exactly in fillet weld UT..
>
> Can you elaborate little bit..
>
> br,
> msms
>
> On Mon, Jan 3, 2011 at 1:40 PM, Sadique Sheikh
>>
>> Dear All,
>> During UT inspection of fillet weld, Does we need both angle probe and
>> normal or TR probe?
>>
>> Thanks & Regards,
>> Mohd. Sadique Sheikh
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
PREM S NAUTIYAL
CELL : 9769316004
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments