Find below attachment table for torque values for different rating of flange. Hope it will fullfill your requirement.
 
 
 
Flange Size Insulated Set Torquing Values @0.15 Standard Torquing Values
F l a n g e   R a t i n g 
150 300 600 900 1500 2500 150 300 600 900 1500
1/2 35 35 35 120 120 120 29 46      
3/4 35 68 68 120 120 120 35 91 91   179
1 35 68 68 192 192 192 40 91 91   287
1 1/4 35 68 68 192 192 285          
1 1/2 35 120 120 285 285 417 52 140 / 160 179   475
2 68 68 68 192 192 285 91 91 113 255 319
2 1/2 68 120 120 285 285 417          
3 68 120 120 192 417 585 113 160 179 319  
4 68 120 192 285 585 1042 102 179 319 626  
5 120 120 285 192 1042 1689          
6 120 120 285 417 792 2565 179   428 695  
8 120 192 417 585 1340 2565 199 287 695 1188  
10 192 285 585 417 2099 5110 255   877 1188  
12 192 417 185 792 2565 N/A 287     1320  
14 285 417 792 792 3692 N/A 428   1188 1563  
16 285 585 1042 792 5110 N/A 380   1563 2233  
18 417 585 1340 1042 N/A N/A 558        
20 417 585 1340 1340 N/A N/A     2010 3195  
24 585 585 2099 2099 N/A N/A     3149 / 2354 5713  
26 585 1340 2099 2565 N/A N/A          
28 585 1340 2565 5110 N/A N/A          
30 585 1689 2565 N/A N/A N/A 780        
32 1042 2099 3692 N/A N/A N/A Conversion Factors
34 1042 2099 3692 N/A N/A N/A To Convert Into Multiply By
36 1042 2565 5110 N/A N/A N/A LBFT (Torque) Nm (Torque) 1.3558
38 1042 1042 3692 N/A N/A N/A LBF / IN2 (Stress) S/mm2 (Stress) 0.008895
40 1042 1340 3692 N/A N/A N/A LBFT (Torque) Kgm (Torque) 0.1383
42 1042 1340 5110 N/A N/A N/A BAR (Pressure) PSI (Pressure) 14.5038
44 1042 1689 5110 N/A N/A N/A LBF (Load) Newtons (Loads) 4.448
46 1042 2099 5110 N/A N/A N/A % STRAIN / STRESS Conversion
48 1042 2099 N/A N/A N/A N/A 0.10% 30000 lbf/in2
50 1689 2565 N/A N/A N/A N/A 0.15% 45000 lbf/in2
52 1689 2565 N/A N/A N/A N/A 0.20% 60000 lbf/in2
54 1689 3692 N/A N/A N/A N/A Hydratight Max. Stress Recommendations
56 1689 3692 N/A N/A N/A N/A Carbon Steels 85% of S.M.Y.S.
58 1689 3692 N/A N/A N/A N/A Stainless Steels 65% of S.M.Y.S.
60 1689 3692 N/A N/A N/A N/A Cupronickels 70% of S.M.Y.S.
  Duplex 65% of S.M.Y.S.
 
Have a nice day through out the year 2011.
 
Pramodh



From: alam <alampravez@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tue, January 18, 2011 2:36:07 PM
Subject: Re: [MW:9310] Bolt Torque Value

Hello Dear,

please find the details, if yuo need code wise i will provide you later.


Thank you

pravez alam

***********************************************************************************


Nom. Fig.Size     Bolting No.    Rec. Bolt     Torque    Torque    Torque
    Ins. (mm)        x Dia. Ins    Stress (lb/in2)    50% (Nm)    80% (Nm)    100%(Nm)
½        (15)    4 x ½"      UNC    40,000    29    46    58
¾.        (20)    4 x ½"      UNC    40,000    29    46    58
1          (25)    4 x ½"      UNC    40,000    29    46    58
1 ½      (40)    4 x ½"      UNC    40,000    29    46    58
2          (50)    4 x 5/8"  UNC    40,000    58    92    115
3          (80)    4 x 5/8"  UNC    40,000    58    92    115
4          (100)    8 x 5/8"  UNC    40,000    58    92    115
6          (150)    8 x ¾"      UNC    40,000    103    164    205
8          (200)    8 x ¾"      UNC    40,000    103    164    205
10        (250)    12 x 7/8" UNC    40,000    164    262    328
12        (300)    12 x 7/8" UNC    40,000    164    262    328
14        (350)    12 x 1"    UN8    40,000    246    394    492
16        (400)    16 x 1"    UN8    40,000    246    394    492
18        (450)    16 x1 1/8"UN8    40,000    286    457    571
20        (500)    20 x1 1/8"UN8    40,000    286    457    571
24        (600)    20 x 1 ¼"  UN8    40,000    400    640    800
30        (750)    28 x 1 ¼"  UN8    40,000    400    640    800
36        (900)    32 x 1 ½"  UN8    40,000    708    1133    1416
















On 1/18/11, Ramesh Barot <rameshnbarot@yahoo.com> wrote:
> Dear All Experts,
>
> Pl. tell me what is the torque value required for  A325 property class 8.8
> M24
> bolt tightening?
>
> What wil be the max. value for it?
>
> Pl. give code reference.
>  Thanks,
> With Best Regards,
> Ramesh Barot
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Pravez Alam
Doha Qatar
Mob#+9746813248

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...