Tuesday, January 18, 2011

Re: [MW:9291] RE: 9281] welder qualification from cs to ss and vice versa

yes you can welding on SS,IF Your welder is qualify with C.S, NOW LATEST ADDENDA OF 2011. IN ASME SEC-IX, WELDER IS QUALIFY FROM    P-N0-1 to P11,P34,P41 TO P49
PLEASE REFER TO ASME SEC-IX AS PER 2011 LATEST VERSON
 
AND ONE THING THAT P No IS CHANGE OF P91 MATERIAL BEFORE THAT THIS MATERIAL P-No is P5B, BUT NOW IS P15E
 
WITH BEST REGARDS
VIKAS KUMAR
ENGINEER-QA/QC
WELDING ENGINEER
Contact Detail:- +91-9650008132 
On Tue, Jan 18, 2011 at 11:13 AM, Vinod Kataria <vinod.kataria@blissanand.com> wrote:

No he cannot weld on SS if qualified on carbon steel.

 

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of krishna
Sent: Tuesday, January 18, 2011 10:17 AM
To: materialswelding
Subject: [MW:9281] welder qualification from cs to ss and vice versa

 

dear all,
                     how a welder qualified in carbon steel can also weld stainless steel and vice versa?

my question is where in ASME sec ix it is given ?

pls clarify

regards,
kk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...