Do you have impact test requirements?
Any how at this temperature you are in the full austenitic range the 1,1 (like in the case of AC3) restriction applies
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Friday, January 7, 2011
Re: [MW:9142] Thickness qualification range for duplex SS with PWHT (ASME IX)
Subscribe to:
Post Comments (Atom)
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...