we have a wps and pqr for p 43 material of inconel, filler wire
incrmo3.But we can use it for
p45 material uns no n08926? this material grop alloy-622 and filler
wire nicrmo-3 both filler wire is same but gtaw process P number is
assencial as per asme sec 9. i have doubt to use it are not
incrmo3.But we can use it for
p45 material uns no n08926? this material grop alloy-622 and filler
wire nicrmo-3 both filler wire is same but gtaw process P number is
assencial as per asme sec 9. i have doubt to use it are not
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.