Saturday, January 8, 2011

[MW:9150] Welding Procedure For P91 Welding to P91 Welding

Dear all,
                  could you please tell me, how can i do the welding on P91 TO P91 MATERIAL,
I WANT TO KNOW THAT ,can i preheat the material with Burner with 250 degree Cel. could you please explain me how can i do the welding on P91,
PLEASE REPLY ME AS SOON AS POSSIBLE, BECAUSE I HAVE NO INDUCTION COIL HEATING MACHINE,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...