This material does not require any preheating

John du Plessis

Technology Manager

 

Tel: +27 (11) 298 2100

Tel: +27 (11) 298 2103 (Direct)

Fax: +27 (11) 836 6014

Mobile:+27  82 883 4970

www.saiw.co.za

 

This email and any files transmitted with it are confidential and may be legally privileged. They are intended solely for the use of the individual or entity to whom they are addressed. Access to this e-mail by anyone else is unauthorised, and any disclosure, copying, distribution or other use of this e-mail is prohibited and may be unlawful. We will not under any circumstances have any responsibility or liability arising out of or in connection with any unauthorised use of this e-mail. If you have received this email in error please notify the sender before deleting it.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Eray Abaci
Sent: 01 October 2010 04:06 PM
To: materials-welding@googlegroups.com
Subject: [MW:7310] About preheating temperature of EN10025 S235JR (1.0038) material

 

Hi dear friends,
Can anybody give me information about what is preheating temperature of S235JR material having 40mm thickness. And also, if there is a calculation, how is calculation for different material's preheating temperature.
Thank you in advance.
Regards.