Yes you can use plate PQR for qualification a pipe WPS as per ASME sect IX provided applicable P number, Group number is within limit.
As per QW 451 table no restriction for pipe diameter
However there is restriction for pipe diameter PQR for certain consrtuction code i.e API 1104
> Date: Mon, 3 May 2010 20:33:25 -0700
> Subject: [MW:5037] Pipe or Plate PQR ?
> From: rmjiran@gmail.com
> To: materials-welding@googlegroups.com
>
> Hi dear all
> Please somebody tell me if I can use a plate PQR for qualification a
> pipe WPS according to ASME Sec. IX?
> I could not find any thing about that in ASME code. If it's possible
> then why there is pipe diameter limit in PQRs?
> Please refer to ASME paragraph.
>
> Thanks
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Catch the changing security environment Get it now.
As per QW 451 table no restriction for pipe diameter
However there is restriction for pipe diameter PQR for certain consrtuction code i.e API 1104
Bharat B. Gole
> Date: Mon, 3 May 2010 20:33:25 -0700
> Subject: [MW:5037] Pipe or Plate PQR ?
> From: rmjiran@gmail.com
> To: materials-welding@googlegroups.com
>
> Hi dear all
> Please somebody tell me if I can use a plate PQR for qualification a
> pipe WPS according to ASME Sec. IX?
> I could not find any thing about that in ASME code. If it's possible
> then why there is pipe diameter limit in PQRs?
> Please refer to ASME paragraph.
>
> Thanks
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Catch the changing security environment Get it now.
Comments