Dear All,

In our project we have requirement of Zinc-Plating / bichromate-treated on bolting in carbon steel & P11 piping class.
Now Max. Design Temp in P11 piping classes is 405 DegC & 200 DegC in carbon steel classes.

I want to know the max temperature upto which zinc plated bolting can be used & if zinc plating is not suitable for this temp other alternative plating type.

Thank you for your kindly help.


Kind Regards,
Vijay Kadam

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...