It is wear resistance material. Only hardness. 

On Mon, 31 Aug 2020 7:57 pm jaimin...@gmail.com, <jaiminthejack@gmail.com> wrote:
Dear Gents,

I got one WPS for  hardox 450 

Required Code: AWS D1.1
Plate Thk: 25mm

My concern is that as per given Data sheet there is not specified Tensile Strength ,on what basis we can accept Report of Tensile Test?

This is my first experience with unlisted material.

Thanks & Regards
Jaimin Patel
B.E Mechanical


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/46b74d37-8ccf-40dd-ab4e-dda0b27073e7n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNLJQnYCG%3DDjraQLZ%2BeCVu2if2c5ro19o34wnxJ3GJ3Ng%40mail.gmail.com.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...