Re: [MW:31373] Unlisted Material AWS D1.1

Request them to furnish Mechanical properties
They will furnish 
No issue at all 

On Mon, 31 Aug 2020, 18:27 jaimin...@gmail.com, <jaiminthejack@gmail.com> wrote:
Dear Gents,

I got one WPS for  hardox 450 

Required Code: AWS D1.1
Plate Thk: 25mm

My concern is that as per given Data sheet there is not specified Tensile Strength ,on what basis we can accept Report of Tensile Test?

This is my first experience with unlisted material.

Thanks & Regards
Jaimin Patel
B.E Mechanical


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/46b74d37-8ccf-40dd-ab4e-dda0b27073e7n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OM-KTP9YMPK2gWcMKsEBAj8uOwvhjw4HuHRpowW4Jn%3Dg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...