This clause is applicable when Notch Toughness  is required in production welding  .
Pl. check the design drawing.
If Design Data is specifying that Notch Toughness Testing  'REQUIRED " then it is required 
Pl. check 
As per my knowledge , for water station piping , it is not required as low temperature application  is not there .
Check the drawing .

On Sun, Aug 30, 2020 at 4:13 PM udaya bhaskar <dusroni@gmail.com> wrote:
Dear Experts,


Please Can you clarify to me the above highlighted point "T limits toughness". 
This point Where is and when is applicable these Supplementary Essential Variables in WPS.
Will This Clause be applicable in water station piping WPS at Gulf countries?
Material : API5L-PSL2




--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3ROgt2d1_hs8pgoZqKd5EUjgd7quAqH8h-8z%2BnBfr2%3Dd0A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NOR65DFbjfVQEvUi7d_CPTaOO%3DM09wX6mbtjr0OGop_w%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...