Re: [MW:31356] As per ASME Sec IX Ed. 2019, ASME Sec VIII, Div-1 and API RP 582

Impact testing is very much required.

On Wed, Aug 26, 2020, 09:47 K K <karan.hbl@gmail.com> wrote:
Dear Experts,  

Impact testing requirements for  Equipment Anchor Chair to top plate/wash welding, base plate, and plug welding.
According to ASME B31.3  above 25mm impact test required.
So for that,  I have restricted to my thickness range 5.00mm to 25.4 mm in WPS.
But Now my requirements for welding Equipment Anchor Chair to top plate/wash welding, base plate, and plug welding.  up to  32.88 mm,
For the 32.88 mm thickness, I have to conduct an impact test or not required impact test 
Process - SMAW.
P No - P1.Gr.No- 1 to P1 Gr,1/2
Thickness range - 5.00 mm to 32.88 mm.
Material - ASTM 516 Gr.60 to ASTM Gr.70

As per ASME Sec IX Ed. 2019, ASME Sec VIII, Div-1, and API RP 582according to mentioned code required Impact test or not?

Thanks in advance  

Regards
KK





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b8875b6c-08f8-4701-9b20-518206a2b1een%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UMqORASPecUf0rqYhUy5gtWZDacOPBoOLqToS0fRmyC%2Bg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...