Re: [MW:31349] How to check Argon Gas Purity?

Dear All

Checking Impurities in Argon gas cylinder is still a secret with the Gas manufacturers.

We need to check following impurities in Ultra high pure Argon gas # CO2, CO, oxide of nitrogen, hydrogen, nitrogen, hydrocarbons, sulphur compounds, mercury, chlorine.

But all Argon gas manufacturers in India are able to check only dew point, moisture and oxygen .

Can anyone help please ..

Regards

Prem Nautiyal
Cell 9769316004

PREM S NAUTIYAL
CELL : 9769316004





From: "PREM SHANKARDUTT NAUTIYAL"<prem_nautiyal@rediffmail.com>
Sent: Sat, 22 Aug 2020 21:14:18 GMT+0530
To: "materials-welding@googlegroups.com"<materials-welding@googlegroups.com>
Subject: Re: [MW:31312] How to check Argon Gas Purity?

Shaw meter will only measure the dew point..

How to measure other impurities like moisture, oxygen, hydrogen, oxides of nitrogen, chlorine, sulphur, etc ?

Regards

Prem Nautiyal

PREM S NAUTIYAL
CELL : 9769316004





From: Kannayeram Gnanapandithan <kgpandithan@gmail.com>
Sent: Mon, 17 Aug 2020 11:33:00 GMT+0530
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:31312] How to check Argon Gas Purity?

Shaw meter available.
But always better weld in a piece and then proceed to job. Due to improper cleaning base metal also will result this black mark

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Aug 17, 2020 at 10:48 AM TRIVIKRAM <trivikram977@gmail.com> wrote:
Dear All,

we are doing Aluminium alloy welding by (TIG) process, during welding we observed black mark around the welding for some argon gas cylinders.

Please suggest how to check the gas purity level and any instruments / gauge are available.

Thanks & Regards,

Trivikram

On Friday, April 4, 2014 at 9:23:35 AM UTC+5:30, prabhu wrote:
Dear All,
 
I my doing work on SS material 316L , ensurinig clean and dust free area and surface but enable to rnsure the Argon gas purity.
please guid me how to ensure the gas .
Or is there any divice to check the Argon gas impurities.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https:roups.google.com/d/msgid/materials-welding/5106e351-0d94-4a13-bcc3-16091e6f8d83o@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https:roups.google.com/d/msgid/materials-welding/CAJzm4ePwCLxPry9MUoHJ_8zRcwPMAP==BHaRVSh-HX75m 346A@mail.gmail.com.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1598245139.S.93642.autosave.drafts.1598245605.19225%40webmail.rediffmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...