Re: [MW:31333] Effect of high delta ferrite FN number (12-13) on welding of SS 304 L material

Delta Ferrite in the range of 12-13 FN will affect during.

1. High temperature operation beyond 350degC
2. Since SS 304L also used at sub-zero temperatures presence of ferrite in the range 12-13 FN will affect the Impact properties
3. Results in formation of Sigma phase as it results in low notch toughness.
4. Affects the General atmospheric corrosion resistance of SS 304L

Some snap shots to support above.

Inline image




On Tuesday, 18 August, 2020, 02:36:11 pm GMT+7, Aakash <harenathjha@gmail.com> wrote:


Hello Expert ,
please explain and also provide relevant documents  about effect of higher delta ferrite on SS 304L materials 

Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fb5b98bf-543e-42eb-8a4e-73dd980cd290n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...