Monday, August 17, 2020

Re: [MW:31322] Essential Variable (SMAW) - Trade Name

No new qualifications is required

On Mon, Aug 17, 2020, 17:46 Gowtham Rajendran <rajgowthamiwe@gmail.com> wrote:
Dear All,

I have a doubt from ASME Sec. IX as mentioned below , please clarify.

Welding Process : SMAW
Electrode used in PQR : E7018-1 (Kiswel)
Toughness Test : Applicable 

So as per Table (QW-253) - QW 404.12 is supplementary essential variable 

Electrode available Now : E7018-1 H4 (Oerlikon) & this has to be used in production now.

Suggest whether the manufacturer of welding consumable can be changed  with same electrode classification or new PQR has to be Qualified.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABLAf1LU2rQ%2BjYBXZp7NyefwaONeHqSH8gxn%3D3NYD5LK%2Bt1Qog%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UP4f89ot1rDGj6y_xEuqowZTmBcYe89P%2BREXR3%2BiDqBsw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...