Thursday, August 13, 2020

Re: [MW:31305] dew point

Apart from nitrogen purging, you have the option for DRYER. 


On Wed, Aug 12, 2020 at 12:35 PM Peter Soloman <petervsoloman@gmail.com> wrote:
In pipeline -20 deg Celcius dew point obtain By nitrogen purging  
or any other way (air compressor and coller
this is check with normal due point meter
Regards,
PETER SOLOMAN
TTSJV -Bahrainmat

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMvP5swwR7qsz90PVxoNx-6JVcuDkKNV1x4Kw0Thnd8DwfC7qg%40mail.gmail.com.


--
 Regards :-
R.NAVANEETHA KRISHNAN,
+968 94332545
+919489556261

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK56KL3Pc79ebw6pqwEjqEjH6q8N_sSHezmws7CSy%3DqJFFtGiQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...