Dear,

 

Yes this statement was issued back in 2015 or 2016 edition of ASTM A 194, please refer the latest version under Section 7.2

 

Best Regards

 

DHANABAL JALACHANDRAN

Senior Inspector | Yanbu Steel Company

CSWIP 3.2.2 & BGAS Gr 2

 

Sent from Mail for Windows 10


On Mon, Aug 10, 2020 at 5:25 PM salim sogec <salimsogec84@gmail.com> wrote:
Dear Gents

Can we use ASTM A194 Grde-7 nus instead of ASTM A194 Grade-4nuts.
Because ASTM A194 Grade-4 nuts removed by the ASTM committee because globally lack of material availability.

Please advise.
Salim

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAH1-07WaQZ6VvLwZmwnf--t%3Dv5iBMmWuAigP1daFbF%2BKdHW%3D4g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPLwtDfnqubdiqt1eM3_AVDQ4%2B0OPvTMznLcupThBhan2P%3Djwg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...