Re: [MW:31296] How to Calulate thickness range of branch connection for welding clearance

I dont understand your question

Στις Τρί, 4 Αυγ 2020, 11:39 ο χρήστης 'Dinesh' via Materials & Welding <materials-welding@googlegroups.com> έγραψε:
Dear experts,
Please see the joint as below,

Here 4"x STD pipe welded with Nozzle #AY,CL150 4"x1" ( branch side thickness is 14 mm)

In as per project WPS,GTAW thickness range 12 mm Max and welder qualified range is 11.08 mm Max.
So in this branch ,how we can calculate thickness range (Like Governing thickness for PWHT) which accept or reject as per project requirement & B31.3 .

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/af652036-0d04-4c79-aa1f-614dc6f73586n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CsREzQ1w--%3DJ7tM%2Bj-S1BKpxWBD-SMWbcg1LAQkRZ5iw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...