Minimum  NDT % is governed by applicable fluid service as per chapter VI of ASME B31.3.
Client can always ask for more stringent requirements.
I am attaching the NDT extent as per chapter VI for quick reference.

Best regards,
ATUL Khatri


On Aug 6, 2020 8:23 AM, "Mr. Sabi" <sabi2kg@gmail.com> wrote:
It is based service and company procedure.


On Wed, Apr 11, 2018 at 2:53 PM Mukul <mukulhossen70@gmail.com> wrote:
Dear Experts,

Can anybody help me by telling the RT percentage in ASME B31.3 ? Is the percentage is mentioned in the code or not ?




Regards,

Mukul Samad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHma%3D444xNCDo1M_Wh3WsAeM1ys%3DNFKBnQo%3D_yN9i-A89CquDg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeCtJr%2BfATbPr4sw_F_W%2BL6d3oyGNqhj3bo%2B7ZUU4m44wg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...