Tuesday, August 4, 2020

Re: [MW:31281] Percentage of RT As Per ASME B31.3

that's right. this is correct answer.

2018년 4월 11일 수요일 오전 9시 49분 29초 UTC-4, perumal govindan 님의 말:

We can't decide this,  Piping  Design / Process Engineering team decides the percentage requirement of RT and indicated the requirements in the piping line list.

I believe we can't simply follow ASME B31. 3.

On Apr 11, 2018 15:49, "Mukul Hossen" <mukul....@gmail.com> wrote:
Ok.I got your point. So for category M fluid service what will be the RT percentage? 

On Wed, Apr 11, 2018, 6:29 PM Perumal Govindan <perumal...@gmail.com> wrote:

Hi Mukul,

It's a project requirement, ASME B31.3 will indicates the fluid service categories.

Percentage of radiography is normally mentioned in the NDT requirements of Client/Welding and NDT Specification.

Also, you can refer project (PMS) Piping material specification / Piping line list / Isometric Drawing.

The requirements are mentioned in the approved line list is the final and follow the same.

Thanks

On Apr 11, 2018 13:53, "Mukul" <mukulh...@gmail.com> wrote:
Dear Experts,

Can anybody help me by telling the RT percentage in ASME B31.3 ? Is the percentage is mentioned in the code or not ?




Regards,

Mukul Samad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/09a63fcb-21bf-4caf-8beb-7bee7b53c468o%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...