Saturday, August 1, 2020

Re: [MW:31248] Photo from Herish Varude

Dear Herish,
Following are the defects seen in attached radiograph:
1. Root side undercut, looks like irregular LF
2. Cavity
3. Image like black wire seems a process mark, will be disappear after reshoot
4. A lot of spatters, arc strike also seen on other part of weld

Thanks,
Best Regards,
Rajnish Dixit

On Friday, 31 July, 2020, 05:03:33 pm GMT+7, HARISH VARUDE <harish.varude02@gmail.com> wrote:


Dear expert,
Please confirm defect name..

From
Herish varude
Mob.No.:-7990746918

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YKLm43ZWepPgjmG6fKhH3eKkqGZiJ7dqy-37Hk1Z5kOf_Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/778150096.7264286.1596252048979%40mail.yahoo.com.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...