Dear All,

we are doing Aluminium alloy welding by (TIG) process, during welding we observed black mark around the welding for some argon gas cylinders.

Please suggest how to check the gas purity level and any instruments / gauge are available.

Thanks & Regards,

Trivikram

On Friday, April 4, 2014 at 9:23:35 AM UTC+5:30, prabhu wrote:
Dear All,
 
I my doing work on SS material 316L , ensurinig clean and dust free area and surface but enable to rnsure the Argon gas purity.
please guid me how to ensure the gas .
Or is there any divice to check the Argon gas impurities.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5106e351-0d94-4a13-bcc3-16091e6f8d83o%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...