[MW:31301] RE: 31300] Change material grade of Nuts

It should not be a problem, unless hardness and other mechanical properties are within the  specified design ranges . Please read this following blog for general guidance.

 

Thanks.

P.Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of salim sogec
Sent: August 10, 2020 10:19 AM
To: materials-welding@googlegroups.com
Subject: [MW:31300] Change material grade of Nuts

 

Dear Gents

 

Can we use ASTM A194 Grde-7 nus instead of ASTM A194 Grade-4nuts.

Because ASTM A194 Grade-4 nuts removed by the ASTM committee because globally lack of material availability.

 

Please advise.

Salim

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAH1-07WaQZ6VvLwZmwnf--t%3Dv5iBMmWuAigP1daFbF%2BKdHW%3D4g%40mail.gmail.com.


Virus-free. www.avg.com

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...