Monday, August 10, 2020

[MW:31300] Change material grade of Nuts

Dear Gents

Can we use ASTM A194 Grde-7 nus instead of ASTM A194 Grade-4nuts.
Because ASTM A194 Grade-4 nuts removed by the ASTM committee because globally lack of material availability.

Please advise.
Salim

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAH1-07WaQZ6VvLwZmwnf--t%3Dv5iBMmWuAigP1daFbF%2BKdHW%3D4g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...