Skip to main content

Re: [MW:29588] Geometric Unsharpness and discountinuity size related to RT

Dear sir, 

I agree with you. 

Please go through the below condition. 
Ug is 0. 2mm

Suppose the actual defect size is 2mm. Then in the radiography films it will show as 2.4mm.

If the upperlimit for that defect as per governing code is 2mm,  will you accept this defect or not?

If the Ug is less, the same defect can be accepted and if Ug is more, the same defect will get rejected. 


Regards, 

Hareesh K V

On Tue, May 14, 2019, 10:51 AM George Dilintas <dilintas@gmail.com> wrote:
There is no specific reference. The Ug is a criterion for accepting RTs and not for accepting of defects. This is self explanatory and thus there is no need for specific Code paragraph 

Στις Πέμ, 9 Μαΐ 2019, 05:40 ο χρήστης Hareesh K V <hareesh13h@gmail.com> έγραψε:
Please give the code reference/clause.

On Wed, May 8, 2019, 6:22 PM George Dilintas <dilintas@gmail.com> wrote:
according to the Code you cannot

Στις Δευ, 22 Απρ 2019 στις 5:28 π.μ., ο/η Hareesh K V <hareesh13h@gmail.com> έγραψε:
Dear Group Members,

Related to : Radiography Examination 

Can we add the value of geometric unsharpness to the discountinuity size acceptability value for accepting a discontinuity. 

Governing codes: 
ASME BPVC Sec V & ASME B 31.3

Example. 

Say Up to 2mm porosity is acceptable as per the code.

We have established the geometric unsharpness value by procedure qualification of the technique and observed as 0.2

My question is, can we accept a porosity of 2.4mm by adding (0.2x 2times Ug for both the sides of the discountiuity) the geometric unsharpness to the acceptability value of 2mm.

Please advise with code references or code interpretations. 

Regards, 

Hareesh K V
8547859202

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CVrfEZAeO2HjLaoz2F1p3pUJH3S7R6EdC-QTL48318yQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAUBHU5O28W2rtbVrBzQMjuCNX0WHwZyW5kXOarcAWtCKw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40DvizPoQheCnG01O0xsSKxUiU__kYdCC5f2gD1ePcTFqw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAX9p8FoL765L%3D%2BwNOgNEj26_fsaay2jKY-2Zsj2Aq7G2w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...