Including fill and cap pass. In a test all are subjected to test

On Sun, 31 Mar 2019 7:56 pm Gowtham Rajendran, <rajgowthamiwe@gmail.com> wrote:
Any increase in heat input above that used in the PQR is not allowed as per AWS D1.1 & ASME Sec IX , when CVN requirements apply , so in this case with max. & min, heat input , how we should fix the max. heat input for filling passes.
On Sun, 31 Mar 2019 at 07:57, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Take minimum and maximum among the reading recorded

On Sun, 31 Mar 2019 8:04 am Gowtham Rajendran, <rajgowthamiwe@gmail.com> wrote:
I.e Heat Input is different in various layers for the fillup passes.

On Sat, 30 Mar 2019 at 18:01, Gowtham Rajendran <rajgowthamiwe@gmail.com> wrote:
Hi ,
       A very good evening to you all.
       My doubt is in establishing the heat input for multipass welding , (root , fill & cap) , for the fillup passes my parameters are different for different layers , which one should i consider for establishing the Heat Input because in this CVN Requirement apply & the heat input cannot be increased as per the code (Be it ASME Sec IX or AWS D1.1).
       How to solve this problem? Kindly help.

Regards,
Gowtham.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...