Saturday, March 30, 2019

Re: [MW:29423] Re: ASME SEC IX Code Issue

You can check EN 1011 - 2 for preheat requirement as well. 

On Fri, Mar 29, 2019, 7:34 AM Souravbohray <ermechsouravbohray@gmail.com> wrote:
i want to know were is given asme sec 9 what will be interpass temprature.is there any value given in code for interpass temp it is given only + 55 c but what temperature we can go +55 c preheating temp given in asme sec 8  

On Tuesday, 14 September 2010 18:13:18 UTC+5:30, limesh M wrote:

Dear All,

Design Code: ASME B31.3     Welding Code: ASME SEC IX

I have a Low temperature carbon steel impact tested PQR with a PWHT range of 600⁰±10⁰C.Is this condition giving an exemption for me on QW406.3 to prepare a WPS with maximum interpass temperature of 200⁰C.

Maximum interpass temperature observed during specimen welding: 140⁰C

 
Regards,
 
Limesh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...