Thanks for your reply, does weld require peening/hammering?
Sent from my iPhone
See my comments.--
On Thursday, March 21, 2019 at 8:36:30 AM UTC+3, Josnit wrote:Dear Experts,We have observed a crack on a roller of material ZG35CrMo (34CrMo4). We want to do weld repair. Could you please advise the below;1. Consumable to be used: Use E8018-B22. Preheat temperature: 150-200 Deg C & maintained during the welding.3. Inter pass temperature: 250 Deg C max4. Any post heating: No specific post heating required.5. Final heat treatment temperature : U didnt specified the thickness & depth of the weld groove you will prepare for the repair. You can consider a temp of 725 Deg C for 2 hrs holding minimum. use a heating & cooling rate of 150 Deg C/ Hr and controlled heating-cooling above 350 Deg C.6. Any special precautions?: Follow above instructions, it will be no issue.Thanks & regardsSandeep KumarMSc. WE, IWE, Research fellow.
On Thursday, March 21, 2019 at 8:36:30 AM UTC+3, Josnit wrote:Dear Experts,We have observed a crack on a roller of material ZG35CrMo (34CrMo4). We want to do weld repair. Could you please advise the below;1. Consumable to be used2. Preheat temperature3. Inter pass temperature4. Any post heating5. Final heat treatment temperature6. Any special precautions?Sent from my iPhone
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.