Friday, March 22, 2019

Re: [MW:29342] S275JR

P nos are grouped based on campetable  chemistry and mechanical properties. 

On Fri, 22 Mar 2019 3:58 am Maha Charu, <usarasu@gmail.com> wrote:
A36 is almost equal to s275 jr, but no proof if documents except Aramco procedure.
If you need to follow sec ix, need new PQR.  s275jr cannot categorise in ASME sec ix. 

On Thu 21 Mar, 2019, 11:06 AM Rathinavel Arumugam, <rathinavel1976@gmail.com> wrote:
S275JR material is not listed in ASME Section IX and it is superior that S235JR.
Hence you have to go for new PQR.

Regards
Rathinavel

On Wed, Mar 20, 2019 at 3:23 PM Saravanan Murugappan <saravananmurugappan@gmail.com> wrote:
Gents,

I have some queries on Subject material ,What is equivalent to S275JR as per SEC IX ?
If it is un assigned material , We can weld WPS qualified already in S235JR to A-106 Grade B or we have to qualify new WPS ?

Regards,
Saravanan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...