Hi,
I am new to this topic. I have to solve the engineering part of doing the calculation.
Here is the statement of problem-->
Take the actual nominate tube and tube sheet material, conduct analysis
mathematically to estimate the joint strength.
ļ§ Conduct analysis to estimate the maximum expansion the tube can take
without affecting the integrity of the tube section. (Check the wall thickness
reduction in %)
ļ§ Once the maximum expansion on tube has been calculated, check the tube
to tube-sheet joint:
ļ· 0.25mm oversized hole with the tube at maximum expansion
ļ· 0.5mm oversized hole with the tube at maximum expansion
ļ· 0.75mm oversized hole with the tube at maximum expansion
mathematically to estimate the joint strength.
ļ§ Conduct analysis to estimate the maximum expansion the tube can take
without affecting the integrity of the tube section. (Check the wall thickness
reduction in %)
ļ§ Once the maximum expansion on tube has been calculated, check the tube
to tube-sheet joint:
ļ· 0.25mm oversized hole with the tube at maximum expansion
ļ· 0.5mm oversized hole with the tube at maximum expansion
ļ· 0.75mm oversized hole with the tube at maximum expansion
Nominal tube diameter-38.1 mm
> Nominal tube sheet hole-38.56 mm
> Nominal tube sheet hole-38.56 mm
tube thickness 3.2 mm
Tube material SS 304
TEMA Extract (values in mm, bracket in inches
38.10 (11/2) Tube nominal dia
38.56 tube sheet nominal dia
(1.518)
0.18 under tolerance
0.08 over tolerance
(0.003)
(1.518)
0.18 under tolerance
0.08 over tolerance
(0.003)
I have calculated maximum expansion of the tube as per the attached excel. Can someone help me to make the calculation for the above statement?
Thanks
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments