Dear experts,
Thanks for your reply,
The roller is in service and we do not have WPS/PQR.
During evaluation it is observed that crack dept is around 25-40mm. 
Total roller thickness is 280mm. 
Sent from my iPhone
Dear Experts,We have observed a crack on a roller of material ZG35CrMo (34CrMo4). We want to do weld repair. Could you please advise the below;1. Consumable to be used2. Preheat temperature3. Inter pass temperature4. Any post heating5. Final heat treatment temperature6. Any special precautions?Sent from my iPhone