Re: Re: [MW:28414] Tack welder qualification

Agreed, there is no seperate qualification for tacks as per UW-31(c) clearly states that the tack welds to be left in place shall be made by welders qualified in accordance with Section IX.

Moreover, if it is temperory tack then it does not mandate to be a holder of code certificate of authorization.

But to be clear with the conclusions, there are no seperate qualification for only tacks.

Regards,
Mohamed Muneeb Mahabobb.



 
Date: 2018-10-10 07:52
Subject: Re: [MW:28413] Tack welder qualification
As per UW 31, it refers section IX for qualification of welders and welding operators. There is no separate category as Tack welders as mentioned in AWS D1.1, 4.15.1.2.
All tack welds and welding shall be made by a Qualified welders( There is no separate category for tack welders in ASME, Piping etc). Hope it is clear


THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ASNT-Level II in PT,MT,RT & UT.
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Oct 10, 2018 at 7:40 AM Prakash Gotimukul <gprakash31@gmail.com> wrote:
UW 31 asme sec viii div 1

Rgds.
Prakash G  AIS

On Mon, Oct 8, 2018, 08:49 sunil kaushik <sunilkaushik08@gmail.com> wrote:
Ok noted but my tack welders are working at fitup section and welders are working at Welding area.my concern is that how I am sure that my tack welder is qualified tack welder.is there any test is required?

On Mon, 8 Oct 2018 at 7:41 AM, Mohamed Muneeb <muneebslsa@gmail.com> wrote:
Also if SA company project then required. 

On Sun, Oct 7, 2018, 5:02 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
What is the code of contruction. If it is AWS D1.1, yes required. But otherwise no. 

On Sun, 7 Oct 2018 3:34 pm SUNILKAUSHIK, <sunilkaushik08@gmail.com> wrote:
Dear sir,
           I am working in fabrication company of piping.My company divided the the welders in two different area-(1) tack welders & (2) welders.Tack welders are working at fitup section & welders are working in welding area.Now my question is that-is it required to qualify the tack welders?If yes then why? If yes than how i will proceed & how to make the prolongation of tack welders?

On Thursday, 15 December 2011 20:22:28 UTC+5:30, samshuddin k wrote:
Dear Sir
Thanks for your guidance.
Still I am not clear with the concept
ASME Sec IX says all welding shall be done by a qualified welder, So
for tacking groove joint,
welder need to be qualified for groove joint.....?
Or if he qualified for fillet joint, he can allowed for tacking groove
joint (Tack either incorporated into the final weld or removed).....?
please reply
Samshuddin.K
Asst Engineer-QSA
N-KOM

On 12/13/11, Morin, Darcy (Bantrel Management Services)
<Mor...@bantrelmanagementservices.com> wrote:
> ASME IX recognizes "Welders and Welding Operators".  There is no provision
> for "Tack Welders" in ASME IX.  However, ASME B31.3 328.5.1(c) mentions
> "Tack Welders", and here is the subsequent Interpretation of this clause:
>
>
>
> Interpretation 22-35
>
> Subject: ASME B31.3-2008, Para. 328.5.1(c), Tack Welding Welder Performance
> Qualifications
> Date Issued: October 5, 2009
> File: 09-1003
> Question (1): Does ASME B31.3, para. 328.5.1(c) require that tack welds,
> whether they are to
> be incorporated into the final weld or be removed, be made by a qualified
> welder?
> Reply (1): Yes.
> Question (2): Does ASME B31.3, para. 328.5.1(c) require that tack welds be
> made to a qualified
> WPS for that joint?
> Reply (2): Yes; see para. 328.5.1(a).
> Question (3): Does ASME B31.3, para. 328.5.1(c) allow tack welds on a groove
> weld joint to be
> made by a welder qualified on a fillet weld test?
> Reply (3): No. See ASME BPV Code Section IX, para. 303.2.
>
>
> Regards,
>
> Darcy Morin
>
> Bantrel Management Services
> mor...@bantrel.com
> o - 780 979 6225
> c - 780 782 5692
>
> -----Original Message-----
> From: material...@googlegroups.com
> [mailto:material...@googlegroups.com] On Behalf Of samshuddin k
> Sent: December 13, 2011 9:49 AM
> To: materials-welding
> Subject: [MW:13203] Tack welder qualification
>
> Dear Experts
> There is any clause in ASME Sec. IX for tack welder qualification.
> Which Code explains tack welder qualification for piping regards
> Samshuddin.K
>
> --
> To post to this group, send email to material...@googlegroups.com
> To unsubscribe from this group, send email to
> materials-weld...@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> This e-mail and any attachments may contain confidential and
> privileged information. If you are not the intended recipient,
> please notify the sender immediately by return e-mail, delete
> this e-mail and destroy any copies.
>
> Any dissemination or use of this information by a person other
> than the intended recipient is unauthorized and may be illegal.
>
> --
> To post to this group, send email to material...@googlegroups.com
> To unsubscribe from this group, send email to
> materials-weld...@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...