Skip to main content

Re: [MW:28427] Can I use WPS/PQR P NO-1, Group NO-1 (PLATE) to P NO-1, Group NO-2 (PLATE) for welding of ASTM A333 Gr.6 (P No: 1, Group No: 1) to ASTM A350 Gr.LF2 CL.1 (P No: 1, Group No: 2) ?

Dear Experts,

We are actually in the process of making WPS for Hot Tapping . in this context while referring to API 1104 , unable to interpret the below paragraph from API 1104 In Service welding .

Kindly help in understanding

B.2.3.1.2 Pipeline Operating Conditions


For in-service welds, an increase in the severity of the pipeline operating conditions (in terms of weld cooling rates)
above the group qualified constitutes an essential variable.

Thanks in advance

Regards,

SRK

On Mon, Sep 17, 2018 at 2:13 PM sandeep kumar <sandeepdhiman63@gmail.com> wrote:
Specific to your query, please see below clause of ASME Section IX.

QW-211 BASE METAL
The base metals may consist of either plate, pipe, or
other product forms. Qualification in plate also qualifies
for pipe welding and vice versa.

Thanks & regards
Sandeep Kumar

On Monday, September 17, 2018 at 1:46:44 PM UTC+3, chiranjeevulu wrote:
Dear Nithin,

My query:

Can I use Plate  PQR (P1 G1 to P1 G2),  for piping welding job (P1 G1 to P1 G2) ? and both PQR with impact requirement.



On Mon, Sep 17, 2018 at 3:34 PM Nithin Joseph <nithind...@gmail.com> wrote:
Hi Please check your query,

You are saying "Can I use WPS/PQR P NO-1, Group  NO-1 (PLATE) to P NO-1, Group NO-2 (PLATE) " if your PQR is P1 G1 to P1 G2, then you can use this PQR for subject application with impact testing.
If your PQR is P1 G1 to P1 G1, then this PQR cannot be supported for welding the subject application.


On Fri, Aug 24, 2018 at 5:58 PM Temburu Chiranjeevulu <chiru...@gmail.com> wrote:
Dear Experts,

1. WPS/PQR (P NO: 1, Group No-1 to P NO: 1, Group No-1 ) is available with contractor

2. Pipe material: ASTM A333 Gr.6 (P No: 1, Group No: 1)

     Flange/Fitting material: ASTM A350 Gr.LF2 CL.1 (P No: 1, Group No: 2)

     WPS/PQR ( P NO: 1, Group No-1 to P NO: 1, Group No-2 ) is not available with contractor 

3.  Charpy "V" notch test to be done

My query is 
 
Can I use WPS/PQR P NO-1, Group  NO-1 (PLATE) to P NO-1, Group NO-2 (PLATE)   for welding of  ASTM A333 Gr.6 (P No: 1, Group No: 1) to ASTM A350 Gr.LF2 CL.1 (P No: 1, Group No: 2) ?

Please give suggestions, Is it possible in accordance with ASME Section-IX  ?



CHIRANJEEVULU TEMBURU l Inspection Engineer-Mechanical I +918790956353.



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Thanks and Best Regards,

CHIRANJEEVULU TEMBURU l Inspection Engineer-Mechanical I +918790956353.
Capacity Augmentation of Jamnagar Loni LPG Pipeline Project of GAIL(JLPL),
GAIL- JAMNAGAR.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...