Thursday, March 1, 2018

Re: [MW:27411] What is this defect

Hi 

First 2 pics looks similar to uniform corrosion and the third is localized corrosion. 

Kind Regards 
Shyamal 

On 1 Mar 2018 3:36 pm, "Guru. Thilakar" <guru.thilakar@gmail.com> wrote:
Dear experts,
                         Which type of painting defect is this i attached the photo anyone please explain. 



Regards,
Guru.G 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone