It is a process of tightening the flanges while the line/flange is in service. normally it is done at very high and low temperature service, when leaks are observed during startup operation.
-- Regards,
Kiran
On Thursday, March 1, 2018 at 8:19:50 AM UTC+3, PK wrote:
On Thursday, March 1, 2018 at 8:19:50 AM UTC+3, PK wrote:
Experts,What is mean by Hot Bolting ?Thank You.