Re: [MW:27108] Qualifications of welders

As per ASME SEC IX QW-350 WELDING VARIABLES FOR WELDERS, most of welding processes 'P' number and 'F' number is essential variable. regardless of other essential variables. There will be a difference in above-mentioned variables for Duplex and S.S. So required Separate qualification.

Please Advice.

Thanks & Regards

PRADEEPKUMAR HORMIS

Mob: +966-58 16 20 710



 
 


 

On Mon, Dec 4, 2017 at 1:47 PM, navnitkumar parikh <parikhnavnitkumar@gmail.com> wrote:
Kindly specify welding process & reference code to answer your query.

Considering ASME  SEC.IX as reference code and welding process as GTAW & SMAW, the answer is YES you can use welder qualified in SS (P No.8) for production welding of DSS (P No.10H) because
1) base metal qualification range is P‐No. 1 through P‐No. 15F, P‐No. 34, and P‐No. 41 through P‐No. 49 (Refer QW-403.18 and QW-423)
2) All F No.6 is qualified for GTAW and all F No.5 is qualified for SMAW (Refer QW-404.15 and QW-433)

Also welder need to meet all essential variables of Table QW-353 for SMAW and QW-356 for GTAW.

Regards,
Navnitkumar Parikh

On Mon, Dec 4, 2017 at 3:51 PM, 'ms viswanathan' via Materials & Welding <materials-welding@googlegroups.com> wrote:
No, because DSS - P number is 10H and A.No-7 and .S.S-   P number is -8 and A.No 8 , essential variables.
 
Regards, M.S.Viswanathan


On Monday, December 4, 2017 12:42 PM, foued oudina <oudinafou21@gmail.com> wrote:


Dear Colleagues ;
 
 
Could you  please help me, we have welders qualified in SS they can weld DSS.
 
Thanks
 
 
 
 
cid:image001.jpg@01D1D9DB.D92C4F40
OUDINA FOUAD | QC Welding OFF PLOT
Técnicas Reunidas Group
TouatGaz Project – EPCC Processing & Production Facilities
Field Engineering Group                   
Oued Zine, Adrar, Algeria
( Ext. 3912
 
 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...