You can take an opening. However, the fitting need to be rechecked for its strength etc as per the ASME code guidelines and this needs to be approved by the client also.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Hareesh K V
Sent: Wednesday, November 22, 2017 5:17 PM
To: materials-welding
Subject: [SOCIAL NETWORK] Re: [MW:27039] Branch connection (Tapping) from a standard fitting

 

Dear Mr.Nisarg Kedar,

 

Why it is not a good engineering practice?

 

Is there any technical reason for the same or code restricts the same?

 

Regards,

 

Hareesh K V

 

On Nov 22, 2017 5:12 PM, "NISARG KEDAR" <nisarg.tuv@gmail.com> wrote:

It's not a good engineering practice

 

On Nov 20, 2017 11:24 AM, "Hareesh K V" <hareesh13h@gmail.com> wrote:

Respected Members,

 

Reference Code: ASME B31.3

 

Can we take a branch connection from a standard fitting (other than using a O'let)?

 

eg: one 1/2" tapping from a eccentric reducer of 3"NBX2"NB.

 

Please guide me with code clause.

 

Regards,

 

Hareesh K V

+91-8547859202

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...