Dear ,

Not required to do additional PQR ( If impact is not required.) Refer QW-424 in ASME SEC IX.

Regards,
CH V Ramana
BVIL




On Wednesday 29 November 2017, 3:45:21 PM IST, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:


Yes.  New PQR

On 28-Nov-2017 5:37 pm, "varun625" <varun.ndt@gmail.com> wrote:
Dear Experts,
I have a WPS qualified as per ASME Sec IX for ASTM A106 with AISI 4130.Now we have a requirement to weld A105 with AISI 4130. As I understand 4130 is unlisted material as per ASME and we need to qualify WPS every time. Kindly confirm the same or advice. Or can I go ahead with same WPS as there is no requirement for Impact testing. 
Thanks in adv.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...