Sunday, November 26, 2017

Re: [MW:27057] Crack after tack welding by using E6013 electrode

Amit just to add more.

E6013 is normally used in structural applications.

Also check the
1. Carbon Equivalent and the required Preheat which has to be used during tacking.
2. Check the thickness and the resultant restraint and the applicable preheat.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Saturday, November 25, 2017, 8:13:54 PM GMT+4, Amit Singh <amit086@gmail.com> wrote:


Dear Experts,

One of my customer is using our E6013 electrode which is highly cellulosic.

He has observed crack after tack welding.

Need some solution for this problem.

Thank you in advance.

Regards,

Amit Singh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.