Sunday, November 26, 2017

Re: [MW:27057] Crack after tack welding by using E6013 electrode

E6013 is Rutile electrode(Titania - Potassium).

Some electrode manufacturer recommend Rebaking of electrodes at 150degC(some where near by)

1. Try baking the electrodes
2. Check the surface condition of the material welded, a slight warming with Preheat torch is recommended.
3. Check the Root Gap for Tacking.


Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Saturday, November 25, 2017, 8:13:54 PM GMT+4, Amit Singh <amit086@gmail.com> wrote:


Dear Experts,

One of my customer is using our E6013 electrode which is highly cellulosic.

He has observed crack after tack welding.

Need some solution for this problem.

Thank you in advance.

Regards,

Amit Singh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...