RE: [MW:27050] Welding after PWHT on SA335 P11 coil

Really Sir, very precise. Thank you so much.

On Nov 23, 2017 8:51 PM, "Thompson, Dennis" <Dennis.Thompson@teaminc.com> wrote:

Per Table UCD-56-4 of Section VIII, Division 1 of the ASME BPVC (for ASME P-No. 4 steels):

1.       For butt welds in pressure barriers, PWHT is required for thicknesses greater than 5/8-inch (16-mm)

2.       For non-pressure attachment fillet welds, PWHT is required for thicknesses greater than 1/2-inch (13-mm)

 

Per Table 132.2 of ASME B31.1 (for ASME P-No. 4 steels):

1.       For butt, groove, & socket welds in pressure barriers, PWHT is required for pipe thicknesses greater than 5/8-inch (16-mm)

2.       For non-pressure attachment fillet welds, PWHT is required for pipe thicknesses greater than 5/8-inch and fillet throat thicknesses greater than 1/2-inch (13-mm)

 

Per Table 132.2 of ASME B31.3 (for ASME P-No. 4 steels):

1.       For butt, groove, & socket welds in pressure barriers, PWHT is required for pipe thicknesses greater than 5/8-inch (16-mm)

2.       For non-pressure attachment fillet welds, PWHT is required for pipe thicknesses greater than 5/8-inch and fillet throat thicknesses greater than 1/2-inch (13-mm)

 

D. Thompson

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of jitendra raghuwanshi
Sent: Thursday, November 23, 2017 5:49 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:27045] Welding after PWHT on SA335 P11 coil

 

As per my knowledege alloy materials of grade P11 & P12 doesnt require pwht if thickness is less than 13mm.

 

On 22 Nov 2017 5:28 pm, "Hareesh K V" <hareesh13h@gmail.com> wrote:

Sir,

 

With proper approvals and procedure you can go for local PWHT.

 

Regards,

 

Hareesh K V

 

On Nov 22, 2017 5:11 PM, "Makrand Sakpal" <makrands9@gmail.com> wrote:

Dears,

 

We have ordered fired heater in which coil material is SA335 P11. Coil size is 6" x SCH 40 (i.e. 6.625" OD x 0.28" THK). These coils are PWHT'd. Issue is, our vendor forgot to weld the thermocouple RF pads on the coil before PWHT. What needs to be done further if we weld the RF Pads on the already PWHT'd coils? Do we need to do PWHT again for that particular joint?

 

Please let us know your opinions.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...